Nanoindentation Testing in the Micrometer Range
FISCHERSCOPE® HM2000 - Fischer Technology, Inc.
Feature packed, user friendly instrumented indentation instrument to measure Indentation Hardness, Indentation Modulus, Hardness in MPa, Vickers and Martens, Elastic Modulus, Creep and much more of coatings and bulk material using the instrumented indentation test according to ISO 14577-1 and ASTM E 2546. For bulk material and coatings thicker than 1 m (0.04 mils).